Common defects in channel steel production
During the production process, channel steel may encounter various quality issues. Below are some common defects:
1.Dimensional Deviations:
Including length, width=100%, thickness, etc., not meeting specification requirements.
2.Surface Defects:
Blister (or scale):Thin, scar-like metal patches on the surface.
Scratches:Surface scoring or gouging.
Pitting and depressions:Uneven surface with small holes or indentations.
Lamination (or delamination):Separation between material layers.
Blistering:Round raised bumps appearing on the surface.
3.Shape Defects:
Twisting:The section is twisted into a spiral shape along its axis.http://www.hnftsteels.com
Bending (or camber/sweep):The section is not straight, either vertically or horizontally.
Underfill (or insufficient fill):The corners or edges of the section are not fully formed or filled out.